- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Plasma power sources eliminate secondary operations
- July 16, 2013
- Product Release
- Plasma Cutting
Victor® Thermal Dynamics® has launched the Ultra-Cut® XT series of power sources for automated plasma cutting. Its cut quality enables parts to go directly from the cutting table to welding, painting, or assembly without secondary operations. The machine delivers ISO Class 3 or better on cuts on any material from gauge to 2 in. thick, reducing bevel and the need for postcut finishing, the manufacturer reports.
On nonferrous materials, the unit uses the Water Mist Secondary (WMS™) process, which incorporates nitrogen as the plasma gas and tap water for shielding. On stainless steel, the WMS process cuts up to 300 percent faster and lowers per-cut cost by 20 percent or more compared to systems that use argon/hydrogen for the plasma gas, says the company.
The machine can cut 1-in.-thick steel at 80 IPM and 2-in.-thick steel at 30 IPM. It employs HeavyCut™ consumables for cutting at 300 and 400 amps. These consumables use a multiple hafnium insert as opposed to a single insert. According to the company, the two-piece tip runs cooler to help extend part life and cut accuracy across the life of the tip, especially when piercing at higher amperages.
Related Companies
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,