- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Our Publications
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Siemens receives ASME award for 3D-printed gas turbine blades
- December 14, 2017
- News Release
- Additive Manufacturing
Siemens has received a Mechanical Engineering Emerging Technology Award from the American Society of Mechanical Engineers (ASME) for its technological achievement with the first successfully 3-D-printed and fully tested gas turbine blades.
In early 2017 Siemens finished its first full-load engine tests for gas turbine blades completely produced using additive manufacturing (AM) technology. The company successfully validated multiple 3-D-printed turbine blades with a conventional blade design at full engine conditions. This means the components were tested at 13,000 RPM and temperatures beyond 1,250 degrees C. Furthermore, Siemens tested a new blade design with a completely revised and improved internal cooling geometry manufactured using the AM technology.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/16/2024
- Running Time:
- 63:29
In this episode of The Fabricator Podcast, Caleb Chamberlain, co-founder and CEO of OSH Cut, discusses his company’s...
- Trending Articles
- Industry Events
16th Annual Safety Conference
- April 30 - May 1, 2024
- Elgin,
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI