Product Engineer, Research and Development
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
All you need to know about the heat-affected zone
It changes the metal and might change the way you approach forming it
- By Andrea Bustreo
- June 28, 2016
- Article
- Shop Management
Most sheet metal cutting techniques are based on localized melting of the material (see Figure 1). The area between the melted part and the unaffected base metal undergoes chemical and structural modifications. It’s called the heat-affected zone (HAZ).
It often can be recognized by a series of brightly colored bands, also visible near welds. Colors, caused by surface oxidation, are an approximate indicator of the temperature the metal reaches (see Figure 2). For example, this table explains the oxidation colors that form on stainless steel Type 1.4301 (AISI 304) when heated in open air:
These colors, also called heat tint, depend on four factors:
- Steel chromium content. This metal increases the material resistance to oxidation, and therefore colors are less intense or their formation is delayed.
- Oxygen level. During welding, usage of protective gas and an electrode coating can reduce the coloration because they partly shield metal from oxidation.
- Surface condition. If the surface is rough, it oxidizes faster, causing darker colors.
- Surface contaminants. Substances like paint, oil, rust, and even fingerprints can alter heat tint, but do not affect the extension of the HAZ.
Steel chromium content. This metal increases the material resistance to oxidation, and therefore colors are less intense or their formation is delayed.
Oxygen level. During welding, usage of protective gas and an electrode coating can reduce the coloration because they partly shield metal from oxidation.
Surface condition. If the surface is rough, it oxidizes faster, causing darker colors.
Surface contaminants. Substances like paint, oil, rust, and even fingerprints can alter heat tint, but do not affect the extension of the HAZ.
In some cases, the HAZ does not cause these colors or even extend farther than the colored area.
What Are the Causes?
The most important factor that influences the creation of the HAZ is thermal diffusivity. Technically speaking, this coefficient depends on thermal conductivity, density, and specific heat of a substance. Materials that show a high thermal diffusivity are able to quickly transfer variations in heat, rather than heat itself.
In other words, if a material demonstrates high thermal diffusivity, it cools faster, and HAZ is reduced. Conversely, lower coefficients mean that the energy cannot be drained quickly, and the HAZ will be wider. For instance, 304A-grade stainless steel has a thermal diffusivity of 4.2 mm²/s, much lower than structural steel (11.72 mm²/s).
From the production process standpoint, the extension of the HAZ depends on three factors: quantity of heat applied, duration of exposure, and area affected . If large amounts of energy are provided for a long time and with wider beams, the HAZ is larger.
This explains the reason that, regardless of the material being cut, any cutting technique causes a different effect:
- Shearing and waterjet cutting do not provoke a HAZ because they do not overheat the sheet metal.
- Laser cutting generates the smallest HAZ among all thermal cutting techniques because it applies heat on a very small area.
- Plasma cutting generates an intermediate HAZ because the plasma pulse is wider than a laser beam. Higher currents allow for a higher cutting speed, reducing the duration of exposure and the width of the HAZ.
- Oxyacetylene cutting generates the widest HAZ of all thermal cutting systems because of the intense heat, slow speed, and wide flames.
What Are the Effects?
Heating caused by the welding or cutting process and subsequent fast cooling result in both chemical and metallurgical alterations. Oxidation is the most noticeable and immediate change, and it is also responsible for the brightly colored bands. A light surface nitriding also can occur, resulting in an increased hardness and decreased weldability of the metal.
Another common effect is corrosion, derived from stainless steel’s sensitive nature. Intense heat causes the precipitation of chromium carbides around the grain boundaries. In these areas, chromium content drops below 10.5 percent, and steel loses its ability to form a passive film and relinquishes its ability to be stainless. The result is the so-called intergranular corrosion. In extreme cases, metal will turn black.
High temperature also can provoke hydrogen embrittlement. Gas diffuses through the metal and creates a strong pressure within the lattice, reducing its tensile strength and toughness. If the hydrogen gas is not removed, it can cause spontaneous cracking even 24 hours after heating.
From a metallurgical point of view, heat generates localized hardening. In some circumstances, austenitic stainless steel can turn into martensitic, increasing its hardness as well as its brittleness. In other cases, heated metal can become weaker.
How to Deal With the HAZ?
The HAZ can alter the sheet metal composition as declared by the rolling mill to a great extent. During forming, the HAZ can make it difficult to manage the bending angle because it becomes impossible to foresee how metal will behave after a heat-intensive cutting process.
One of the affected behaviors is springback. To get consistent angles with varying elastic recovery, it’s useful to rely on a laser- or contact-based angle control system often found on modern press brakes. Laser-based systems are quite common but have problems working with small flanges and with rough or polished surfaces. Contact systems are more precise and work well with counterbends and small flanges. However, they have a slightly reduced angle span when compared to the laser-based systems.
Imprecise crowning is the other culprit. Every cut piece is different, and the machine frame is stressed in an unpredictable way. For this reason, it’s important to use a press brake with a real-time crowning system, which makes it able to compensate for the machine deformation. This technology helps the press brake obtain regular angles along the entire length of the profile.
Heat tint caused by oxidation can be removed with fine sandpaper or ground away. This exposes the underlying layer and activates chromium self-passivation, but may lead to a weakening of the part.
The only way to remove the entire extension of the HAZ is to machine it away, but that comes with the price of reduced material yield and more labor and machine time required to address the problem area.
About the Author
Related Companies
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/16/2024
- Running Time:
- 63:29
In this episode of The Fabricator Podcast, Caleb Chamberlain, co-founder and CEO of OSH Cut, discusses his company’s...
- Trending Articles
Tips for creating sheet metal tubes with perforations
JM Steel triples capacity for solar energy projects at Pennsylvania facility
Are two heads better than one in fiber laser cutting?
Supporting the metal fabricating industry through FMA
Omco Solar opens second Alabama manufacturing facility
- Industry Events
16th Annual Safety Conference
- April 30 - May 1, 2024
- Elgin,
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI