Analyzing tubes, lubes, dies, and friction

October 10, 2002 | By Dr. Ghafoor Khodayari, Dr. Jean Reid, Mark Garnett

Comparing and correlating two tests, a common bench test (twist compression) and a straight-tube corner-fill test, simulate hydroforming to find the coefficient of friction.