- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Our Publications
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
AMADA WELD TECH Inc.
Recent Content on The Fabricator for AMADA WELD TECH Inc.
- From The Fabricator
Three AMADA WELD TECH technical centers offer sample processing, training
- Jul 14, 2023
- Shop Management
- News Release
AMADA WELD TECH Inc., a manufacturer of welding, marking, cutting, sealing, and bonding equipment and systems, is now processing samples and providing product and process training in three technical centers across the U.S.
- From The Fabricator
AMADA WELD TECH’s galvo scan heads made for precision laser welding
- May 30, 2023
- Laser Welding
- Product Release
AMADA WELD TECH has introduced a line of galvo scan heads for precision laser welding applications.
- From The Fabricator
A resistance weld process monitoring Q&A
- By Mark Boyle
- Dec 20, 2022
- Assembly and Joining
- Article
Weld monitors can help you find the cause of resistance welding problems and provide valuable data for AI and machine learning.
- From The Fabricator
Amada Miyachi America changes company name to Amada Weld Tech
- Apr 6, 2020
- Laser Welding
- News Release
Amada Miyachi America Corp., a manufacturer of welding, marking, cutting, and micromachining equipment and systems, has changed its name to Amada Weld Tech Inc. Amada Miyachi America has been part of the Amada Group since March 2013. The name change is intended to enhance the company’s...
- From The Fabricator
Amada Miyachi America’s WL-300A laser workstation is configurable for industrial manufacturing
- Dec 21, 2019
- Laser Cutting
- Product Release
Amada Miyachi America Inc. has introduced the WL-300A laser processing workstation, configured for nanosecond pulsed fiber laser applications. This workstation is a larger version of the LMWS laser marker workstation, designed to accommodate larger parts. Integrated with the company’s LMF fiber...
- From The Welder
Amada Miyachi America’s MM-400A desktop resistance weld checker monitors key welding variables
- Feb 22, 2019
- Arc Welding
- Product Release
Amada Miyachi America has introduced the MM-400A desktop resistance weld checker. It allows operators to monitor and manage key welding variables that result in changes in weld heat, including current, voltage, time, force, and displacement. The compact unit supports AC, DC inverter, AC inverter,...
- From The Welder
Amada Miyachi America DC2013-T spot welding power supplies offer real-time SPC
- Jan 28, 2019
- Arc Welding
- Product Release
Amada Miyachi America Inc. offers the DC2013-T series resistance spot welding power supply, manufactured by sister company MacGregor™. The system combines touch-panel integrated database process control and monitoring with ultrahigh-duty and low-ripple 3,000-ADC output. The power supply employs...
- From The Fabricator
Amada Miyachi America offers MacGregor DC1013-T and DC613-T spot welding power supplies
- Jan 15, 2019
- Assembly and Joining
- Product Release
Amada Miyachi America Inc. offers MacGregor™ DC1013-T and DC613-T linear DC resistance spot welding power supplies for butt welding fuses, welding components to lead frames, gold ribbon bonding, and welding fine wire to pads. High-speed automation and communication ports offer users full...
- From The Welder
Amada Miyachi America expands Detroit area technical center
- Nov 7, 2018
- Laser Welding
- News Release
Amada Miyachi America, Inc., a Monrovia, Calif.-based manufacturer of resistance welding, laser welding, marking, cutting, and micromachining equipment and systems, has expanded and enhanced its Detroit technical center. The updated facility now features 5,500 sq. ft. of laboratory space devoted to...
- From The Fabricator
Amada Miyachi America’s KN-II pneumatic weld head suitable for opposed electrode welding
- Sep 19, 2018
- Assembly and Joining
- Product Release
Amada Miyachi America Inc. offers the KN-II series pneumatic weld head for opposed electrode welding applications that require fast follow-up to prevent material expulsion. It also is suitable for welding ring or annular projections with a perimeter length from 0.40 to 7.0 in. and for...
- From The Welder
Amada Miyachi America hires southern regional sales manager
- Aug 2, 2018
- Laser Welding
- News Release
Amada Miyachi America Inc., Monrovia, Calif., a manufacturer of resistance welding, laser welding, marking, cutting, and micromachining equipment and systems, has announced the appointment of Stephen F. Shea as southern regional sales manager. He provides sales and technical support for all...
- From The Fabricator
Amada Miyachi America expands Detroit technical center
- Jul 12, 2018
- Shop Management
- News Release
Monrovia, Calif.-based Amada Miyachi America, a manufacturer of resistance welding, laser welding, marking, cutting, and micromachining equipment and systems, has expanded and enhanced its Detroit technical center. The updated facility now features 5,500 sq. ft. of laboratory space devoted to...
- From The Welder
Amada Miyachi America appoints VP of sales
- May 22, 2018
- Laser Cutting
- News Release
Amada Miyachi America Inc., Monrovia, Calif., a manufacturer of resistance welding, laser welding, marking, cutting, and micromachining equipment and systems, has appointed Kurt A. Tolliver as vice president of sales. A 20-year veteran of the company, he previously managed its southern U.S.,...
- From The Fabricator
Amada Miyachi America’s IPB-5000A-MU inverter resistance welding power supply offers output to 6,000 amps
- Feb 15, 2018
- Assembly and Joining
- Product Release
Amada Miyachi America offers the IPB-5000A-MU inverter resistance welding power supply. It features a modified back panel that accommodates most of the company’s weld heads. When paired with the ITB-780A6 transformer, the power supply has a maximum output of 6,000 amps, making it suitable for...
- From The Welder
Amada Miyachi America completes ISO 9001 recertification process
- Oct 9, 2017
- Laser Cutting
- News Release
Amada Miyachi America Inc., manufacturer of resistance welding, laser welding, marking, cutting, and micromachining equipment and systems in Monrovia, Calif., has completed the ISO 9001 recertification process for its quality management system. As part of recertification, the company validated each...
Products/Services
- MarkingLaser Marking Systems
- Welding and JoiningPower Sources – Resistance Welding