Timken Latrobe Steel completes upgrade

April 28, 2005

Timken Latrobe Steel today held an inaugural ceremony to launch the upgraded continuous rolling mill at its Latrobe, Pa. plant.

The mill is equipped with electric induction and resistance heating and uses a three-roll configuration throughout its finishing train.