Ice Industries Grenada will invest $500,000 in an expansion at its Grenada, Miss., plant that will result in the creation of 35 jobs.The company is expanding engineering, testing, and manufacturing at the metal stamping facility, which makes parts for automobiles, appliances, and heating and cooling equipment.