Digital joining process control system enhances welding automation


July 13, 2004

Servo-Robot offers its new DIGI-I joint-tracking system for welding automation. The system uses the latest laser vision technologies to facilitate global process monitoring and weld quality control.

The seam-tracking system features joint-profile monitoring functions, keeping the weld wire accurately positioned in the joint and offering adaptive welding parameter control based on joint variation. It features weld pool, arc sound, and welding parameters monitoring capabilities.

Suitable for robotic, tank and vessel, pipe and tube, and ship panel line arc welding, the system also monitors the weld quality after welding.