Metal print coat finish system offers zinc options


July 31, 2013

Centria has added four new zinc finish options to its Allusion print coat system. The system simulates natural finishes, including wood and specialty metals, using print coating technology.

The finishes — blue zinc, red zinc, crystal zinc, and green zinc — can be applied to both steel and aluminum substrates. They are available on the company's Formawall®; Profile Series Concept Series®, IW series, and exposed fastener panels; and FormaBond® wall panel products.

Other finishes include light oak, dark oak, rust, slate, and antique bronze.