June 13, 2006
The OL200 oxyfuel lifter from MG Systems and Welding is suitable for use with the ALFA oxyfuel torch and provides 150-IPM vertical speed.
The lifter provides increased part accuracy as a result of accurate height sensing through integration with the torch's height sensing system, the company says. Precision ball screw and dual linear guides provide a smooth and rigid platform for vertical positioning of the torch. Sealed bearings require little to no maintenance.
The lifter is also suitable for use with TurboFlame oxyfuel torches on some machine models.