Advanced Machine & Engineering Co. (AME) offers the AMSAW® S300, a sawing system designed to cut both ferrous and nonferrous materials. It has a capacity of 3 to 12 in. and uses saw blade diameters from 24 to 36 in.

The system allows for cut lengths up to 30 in. and multi-indexing when length exceeds 30 in. Accuracy for length is ±0.005 in. The spindle motor is 60 HP/45 kW.

The compact design incorporates hardened spindle gears with minimum backlash. It uses cermet or carbide-tipped, disposable or grindable saw blades. Unattended sawing is possible with the automatic bar-loading table.