March 5, 2010
Fischer Technology has announced the availability of a Bluetooth® interface for its DELTASCOPE® FMP30, ISOSCOPE® FMP30, and DUALSCOPEr® FMP40 coating thickness instruments. The Bluetooth module enables data transmission to a distance of more than 30 ft. for documentation.
The hand-held coating thickness gauges come with a selection of interchangeable probes with wide measurement capabilities.
Bluetooth also is available on the FERITSCOPE® FMP30, which has a plug-in-type smart probe and is suited for nondestructive measurement of ferrite content on-site or in the lab, according to the magnetic inductive method.