- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Arc Welding 101: CV or CC - What’s the difference?
- By Paul Cameron
- Updated February 13, 2023
- May 9, 2014
- Article
- Arc Welding
Q: What is the difference between constant current and constant voltage?
A: I’m often called on to explain this topic when I teach. Electric arc welding has two main variables: current and voltage. Welding machines will supply both, but they are capable of consistently maintaining only one of those variables, while the other is maintained by some other means.
Direct-current (DC) power supplies can be constant-voltage (CV) or constant-current (CC). CV equipment, typically used for semiautomatic and wire-fed processes like gas metal arc welding (GMAW) or flux-cored arc welding (FCAW), provides a consistent preset voltage. Presetting the weld voltage on a CV power supply will maintain a constant arc length, because arc length is directly related to weld voltage.
So what determines the current draw? On CV equipment the wire feed rate, wire diameter, and electrode stick-out draw current from the machine. Set at 28 V, your GMAW or FCAW equipment will set an arc length that will remain constant. As you increase wire feed speed or wire diameter, you will increase your welding current. By increasing current, you increase penetration. On the other hand, maintaining that wire feed speed and increasing electrical stick-out introduces resistance into the electrode and reduces current, thereby reducing penetration.
To avoid burn-through, you will increase stick-out, which reduces current and penetration. You can easily reduce weld current 25 to 50 amps simply by increasing stick-out.
CC equipment, typically used for manual welding processes such as shielded metal arc welding (SMAW), provides a consistent preset current. A CC power supply with a preset current will maintain that amperage setting.
So what determines the voltage? Remember what I said previously about voltage being directly related to arc length? You regulate voltage manually during SMAW or GTAW. By moving that stick or tungsten electrode closer to or farther from the work (generally speaking, less is best).
About the Author
Paul Cameron
Braun Intertec
4210 Highway 14 East
Rochester, MN 55904
About the Publication
subscribe now
The Welder, formerly known as Practical Welding Today, is a showcase of the real people who make the products we use and work with every day. This magazine has served the welding community in North America well for more than 20 years.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Trending Articles
Aluminum MIG wires offer smooth feeding, reduced tangling
The role of flux in submerged arc welding performance
Three ESAB welding machines win Red Dot Awards for product design
Power source added to cobot welding system for simplified automation
Connecticut students compete in Maritime Welding Competition
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,