- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Our Publications
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Flashforge’s new 3D printer runs engineering-grade filaments
- May 10, 2022
- Product Release
- Additive Manufacturing
The FlashforgeUSA Creator 4 3D printer can be fitted with an extruder intended for flexible, engineering-grade, or carbon-fiber-composite filaments.
The desktop printer’s twin extruders work independently or simultaneously. The thermally controlled, 400- by 350- by 500-mm build chamber maintains a constant temperature of 65 degrees C, which effectively reduces model shrinkage, warping at corners, and breakage, reports the manufacturer.
The company adds that linear-rail leadscrew stepping along the X and Y axes improves motion stability and the new S-type motion-control system ensures smooth starting and stopping, precise nozzle positioning, and sharp print details.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/16/2024
- Running Time:
- 63:29
In this episode of The Fabricator Podcast, Caleb Chamberlain, co-founder and CEO of OSH Cut, discusses his company’s...
- Trending Articles
- Industry Events
16th Annual Safety Conference
- April 30 - May 1, 2024
- Elgin,
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI