- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Our Publications
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Xspee3D printer from Spee3D produces metal parts anywhere
- October 24, 2022
- Product Release
- Additive Manufacturing
Spee3D has unveiled its Xspee3D printer, a containerized, ruggedized, and deployable cold-spray metal 3D printer that provides all of the necessary functions to print metal parts from anywhere in minutes, the company reports.
Designed based on extensive field work and collaboration with the Australian Army, the machine is transportable as a standard shipping container with the printer and auxiliary equipment in one box. The printer requires only a connection to electrical power, and once it is live, it can begin fabricating parts immediately.
According to the manufacturer, the printer is 1,000 times faster than other additive manufacturing options and can print one or multiple parts simultaneously from more than 12 metal alloys, including copper, stainless steel, titanium, high-strength aluminum, and nickel-based carbides.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,