- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Our Publications
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Content about Greer Steel Co., A Division of Greer Industries - Page 2
- From The Fabricator
Greer Steel appoints Dover plant engineer
- Apr 12, 2005
- Metals/Materials
- News Release
Greer Steel has appointed Robert L. Bates as plant engineer of the company's Dover, Ohio, facility. A registered professional engineer, Bates has more than 24 years' engineering experience. His experience includes a 12-year position as a plant engineer with MSC Walbridge Coatings and a six-year...
- From The Fabricator
Greer Steel appoints marketing vice president
- Mar 8, 2005
- Shop Management
- News Release
Greer Industries has appointed Bob Friend as vice president of marketing. He is responsible for developing new market opportunities with a particular focus on marketing efforts for Greer Steel and Greer Lime. Friend has a degree in business administration from Louisiana State...
- From The Fabricator
Greer Steel announces key management appointments
- May 4, 2004
- Metals/Materials
- News Release
Greer Steel, a cold-rolled strip steel producer, has appointed Todd Daenzer as vice president, quality and technology; Don Fleeher as vice president, purchasing; and Paul Eagle as vice president, service center operations. Daenzer has been with the company for nine years in various positions,...