FAB-PAK FT-SS
Specifications
Workcell | FAB-PAK FT-SS |
Robot(s) | 100iD |
Robot Reach (In.) | 56 |
Positioner Type* | Single or Dual Zone Fixed TT |
No. of Axes - Robot | 6 |
No. of Axes - External | |
Positioner Load Capacity per Side (Lbs.) | 2,000 |
Workcell Footprint (Ft.) | 9.5 x 7.75 x 8.25 |
Welding Process - GMAW | |
Welding Process - GTAW | |
Welding Process - Laser | |
Welding Process - Spot | |
Welding Process - Plasma | |
Welding Process - FCAW | |
PC-Based Software | |
Maximum Part/Tool Size (In.) | 96 x 36 |