- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
JF2220-GY welding jacket from Black Stallion is NFPA-certified
- August 29, 2018
- Product Release
- Safety
Black Stallion® has introduced the JF2220-GY flame-resistant (FR) cotton welding jacket, certified to NFPA 2112 and NFPA 70E to help protect welders from potential short-duration flash fire and arc flash hazards.
Constructed of 9-oz. FR-treated cotton, the jacket meets ASTM F1506 requirements for flame resistance and is tested to maintain protection through 100 home washings or 50 commercial laundry cycles. Flame resistance is enhanced with strong FR aramid threads throughout the jacket.
Six front snaps on the jacket are covered with a layer of FR cotton to eliminate conduction of electricity in the event of an arc flash incident. These six front snaps are reinforced with leather backing to reduce the risk of tearing and eliminate pull-through.
Features include a standup welder’s collar to protect the neck from sparks and debris, an outside scribe pocket on the left sleeve, and an inside pocket. The extended 32-in. length offers additional torso protection.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/07/2024
- Running Time:
- 67:38
Patrick Brunken, VP of Addison Machine Engineering, joins The Fabricator Podcast to talk about the tube and pipe...
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,