- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Our Publications
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Sawing - Page 22
- From The Fabricator
Mid Atlantic Machinery to host Machine Tool Madness show
- Feb 2, 2012
- News Release
Mid Atlantic Machinery will host the Machine Tool Madness show at its Harrisburg, Pa., showroom March 28-29 for welders and fabricators interested in rolling, robotic welding, eliminating secondary operations, and improving bending techniques. Manufacturers at the show will include TRUMPF,...
- From The Fabricator
Everett Industries names Pacific Northwest sales rep
- Jan 30, 2012
- News Release
Everett Industries Inc. has hired Douglas Clay as sales representative for the Pacific Northwest region, representing the company's abrasive cutoff saws and wheels.
Clay has many years of sales and service experience in machines, tooling, and related metal fabrication products.
- From The Fabricator
Double-column mitering band saw designed for structural, solid, and difficult materials
- Jan 26, 2012
- Product Release
Kalamazoo Machine Tool's model H6A-NC double-column mitering band saw is a fully automatic machine designed for the production of structural, solid, and difficult materials. The machine is fully programmable to enable serial cutting of various lengths, sizes, blade speeds, and quantities and to...
- From The Fabricator
Hole saws, reciprocating saw blades introduced
- Jan 9, 2012
- Product Release
The M.K. Morse Co. has introduced the Morse Diamond Grit™ line of hole saws and reciprocating saw blades.
The products use brazed industrial diamond grit to cut cast iron and other abrasive construction materials.
- From The Fabricator
Manual metallurgical saw features enclosed wet-cutting area with dual coolant nozzles
- Jan 9, 2012
- Product Release
Kalamazoo Industries offers the model K12-14MS manual metallurgical saw. It features an enclosed wet-cutting area with dual coolant nozzles to eliminate the dispersion of abrasive particles into the workplace. The saw has a 14-in. abrasive wheel; a 5-HP, three-phase, 1,725-RPM TEFC motor; dual...
Minimal footprint band saws designed to meet daily production requirements
- Dec 20, 2011
- Product Release
Peddinghaus Corp. offers Eco-Line band saws for cutting steel. Designed to meet daily production requirements, the saws work quickly and efficiently and have a minimal footprint, the company reports. The saws can cut at 30-, 45-, 90-, and 135-degree angles. They facilitate the integration of...
- From The Fabricator
DGI Supply acquires Tru-Cut, Supreme Saw
- Dec 6, 2011
- News Release
DGI Supply, a DoALL Company in Wheeling, Ill., has acquired Tru-Cut Tool and Supply Co. of Alsip, Ill., and its subsidiary, Supreme Saw & Service Co. Inc. Greg Muntean, owner of Tru-Cut, remains with the company as director of business development for DGI’s Sawing Products division. DGI...
- From The Fabricator
Circular saw blades suitable for cutting light- and heavy-wall tubes, extrusions, plates
- Nov 7, 2011
- Product Release
Forrest Mfg. offers circular saw blades for cutting nonferrous metals such as copper, aluminum, and brass. They are suitable for cutting light- and heavy-wall tubes, extrusions, and plates. According to the company, the blades produce burr-free cuts that eliminate the need for filing. Nineteen...
- From The Fabricator
Less lubricant results in better sawing?
- By Tim Walker
- Nov 7, 2011
- Article
For fabricators looking to reduce the amount of lubricant they use for sawing applications, lubricants designed for near-dry sawing may be the answer. These minimum quantity lubricants, as they are called, are designed to provide complete coverage of the blade with as small an amount as possible.
- From The Fabricator
DoALL names new executive at Continental Machines
- Oct 24, 2011
- News Release
DoALL Co., Wheeling, Ill., has hired Kurt Plechaty as executive vice president in charge of plant operations at Continental Machines. An engineer, Plechaty has a master’s degree in organizational leadership and quality. Located in Savage, Minn., Continental Machines manufactures band saws under...
- From The Fabricator
Behringer Saws adds sales manager for Southwest
- Sep 19, 2011
- News Release
Behringer Saws Inc., Morgantown, Pa., has announced that Kyle Adams has joined its sales team as the Southwest regional sales manager. His territory is Texas, New Mexico, Oklahoma, Arkansas, Louisiana, Mississippi, Tennessee, and Alabama. Adams previously worked for Heyco Products and for six...
- From The Fabricator
Three-axis drilling, marking, sawing machine introduced
- Jul 25, 2011
- Product Release
Knuth Machine Tools USA Inc. has introduced the new BeamCenter CNC 1200 saw and drill press center. It offers centrally controlled, customizable beam production, performing simultaneous three-axis drilling, marking, and sawing. The machine features four station tool changers per drill spindle,...
- From The Fabricator
Vertical column saw designed for nonproduction applications
- Jul 11, 2011
- Product Release
The Kalamazoo Machine Tool model C315/350 hinge-type vertical column saw is designed for nonproduction applications requiring cuts in tubes, pipes, and light structural shapes. The saw has a 14-in. blade, 3.5-HP motor, spindle speeds of 24 to 105 RPM with an infinitely variable option in...
Automatic tube saw operates as stand-alone unit or part of processing line
- Jun 20, 2011
- Product Release
The TC720 automatic tube saw from BLM Group USA is designed to operate as a stand-alone unit or as part of a fully automated tube processing line controlled by a single CNC. The programming system has an applications-tested database that covers blade speeds and feeds for different materials,...
- From The Fabricator
Wet benchtop saw measures 24 in. in all dimensions
- May 31, 2011
- Product Release
Kalamazoo Industries' model K10WBT enclosed, wet cutting, benchtop abrasive saw offers manual operation. The 10-in.-dia. abrasive blade (not included) allows the machine to cut up to 1.5-in. solids and 2.5-in. pipe. The saw features a magnetic switch; an internal worklight; dual 3-in. vises;...
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/16/2024
- Running Time:
- 63:29
In this episode of The Fabricator Podcast, Caleb Chamberlain, co-founder and CEO of OSH Cut, discusses his company’s...
- Trending Articles
Tips for creating sheet metal tubes with perforations
Supporting the metal fabricating industry through FMA
JM Steel triples capacity for solar energy projects at Pennsylvania facility
Zekelman Industries to invest $120 million in Arkansas expansion
How welders can stay safe during grinding
- Industry Events
16th Annual Safety Conference
- April 30 - May 1, 2024
- Elgin,
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
- Upcoming Webcasts
Navigating Change: The Manufacturer’s Guide to Change Management with ERP Implementation
- May 16, 2024
- Sponsored
- Presented By: ECI Software Solutions, M1