- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
IDTEchEx report reveals how nickel is replacing cobalt in electric vehicles
- October 12, 2020
- News Release
- Electric Vehicles
Electric vehicle (EV) powertrains are much more materially diverse than the internal combustion engines they replace. As a result, they are putting sudden and unprecedented strain on several raw materials industries.
One of the most crucial materials is nickel, an essential part of the cathode in the lithium-ion batteries enabling electrification. Most automakers use nickel-based batteries for their balance of energy and power density: BMW, Hyundai, and Renault use variants of the lithium-nickel-manganese-cobalt oxide (NMC) chemistry, while Tesla uses a lithium-nickel-cobalt-aluminum oxide (NCA) chemistry. China also now favors NMC chemistries, having phased out lithium-iron-phosphate chemistries.
In 2019 more than 95% of new electric passenger cars sold used a variant of either NMC or NCA, as detailed in the new IDTechEx report, “Materials for Electric Vehicles 2020-2030.” Demand for nickel is further amplified by the trend toward higher nickel content in cells, as manufacturers switch to chemistries like NMC 622 or 811 over the previous 111 and 523 to improve energy density further and reduce dependence on cobalt.
Nickel is the most expensive material in EV batteries after cobalt and also is one of the most highly used outside of the battery industry. While nickel is not discussed as much as cobalt or lithium, sustainable and environmentally conscious supply is becoming more of an issue.
In 2017 the Philippines government suspended nearly half of its nickel mines, citing environmental concerns. Moreover, Indonesia accounts for the largest supply of nickel and in 2019 the country banned exports of raw nickel ore to boost its domestic processing industry. Indonesia also has the most planned developments for increasing nickel production and is set to dominate the supply chain.
Nickel typically is mined from ores that contain only a very small percentage of useful nickel, resulting in a large amount of waste material. Recently two nickel mining companies in Indonesia announced plans to use deep-sea disposal for the raw material waste into the Coral Triangle as they ramp up operations. Less than 20 nickel mines worldwide use deep-sea disposal, but these new facilities would account for millions of tons of waste material each year. This method typically is used because it is cheaper than the alternatives of dam storage or converting the raw materials to useful products.
Many automakers are aware of the environmental concerns in nickel supply and that it can undermine the environmentally friendly message of the EV. Most, including PSA, VW, and Tesla, have pledged to reduce the environmental impact of their batteries. This becomes challenging as the choice of suppliers that can meet the demands of these large automotive companies is limited. In the future nickel producers will have to prove that their practices are environmentally friendly if they want to sell into the European and American markets, where the automotive industry is making this a priority. Elon Musk has been quoted in Financial Times as saying that Tesla would give a “giant contract” to any companies that could mine nickel “efficiently and in an environmentally sensitive way.”
As the EV market grows with the trend toward higher-nickel chemistries, IDTechEx expects the demand for nickel from EV batteries to increase tenfold by 2030 compared to 2019. This makes the environmentally conscious supply of nickel a serious issue going forward for the EV market.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/16/2024
- Running Time:
- 63:29
In this episode of The Fabricator Podcast, Caleb Chamberlain, co-founder and CEO of OSH Cut, discusses his company’s...
- Trending Articles
Capturing, recording equipment inspection data for FMEA
Tips for creating sheet metal tubes with perforations
Are two heads better than one in fiber laser cutting?
Supporting the metal fabricating industry through FMA
Omco Solar opens second Alabama manufacturing facility
- Industry Events
16th Annual Safety Conference
- April 30 - May 1, 2024
- Elgin,
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI