Senior Editor
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Pi and K factors: The mathematical beauty of sheet metal
- By Tim Heston
- July 10, 2012
Sure, my classmates gave him the expected groans, but when I think back to that statement, I know we need more teachers like him. Even in this economy, manufacturers crave people who don’t get scared by adding and subtracting three or four places to the right of the decimal point. Operating a press brake, you basically work with a bunch of triangles (V die opening and bend angles) and degrees of a circle (bend radii). Algebra and (especially) geometry and trigonometry are everywhere.
A recent story on National Public Radio told how manufacturing jobs now require more math skills. I think it’s more accurate to say that the manufacturing jobs that are left happen to require a solid math background--and thousands of those jobs remain unfilled today, even in this economy. Also, it’s not as if metal fabrication jobs didn’t require math decades ago. In fact, you could argue those jobs actually required more math skill. Some shop leaders today have told me how they remember days (sometimes fondly) of manual flat layout, when they took out the slide rule and did it all by hand.
Today software and modern machine tools can automate much of the math, but I think the equations still matter. It’s really the grammar of metal fabrication. For decades, experienced press brake operators have known that a K factor, or bend deduction, is two times the outside setback (or X factor) minus the bend allowance. Some operators even knew that the bend allowance (length of the bend’s neutral axis) can be revealed by multiplying the complementary bend angle by several factors, including such cryptic numbers as 0.017453, which is pi divided by 180, essentially converting numbers to degrees around a circle.
Sure, even before modern software, operators looked at bend deduction charts and learned a lot by doing, paying attention to the experienced guys who knew the trade. But I feel that knowing the math really reveals the straightforward logic of sheet metal forming and fabricating. Material variables--be they varying grain directions or different heats--will always add a dash of unknowns.
But unlike so much in life, metal forming’s foundation is rooted in mathematical truths that, compared to the trials and tribulations of everyday life, are extremely predictable. Mix this scientific predictability with the wild ride of running a contract metal fabrication business, and you’ve got a thing of beauty that’s both chaotic and rational at the same time.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscriptionAbout the Author
Tim Heston
2135 Point Blvd
Elgin, IL 60123
815-381-1314
Tim Heston, The Fabricator's senior editor, has covered the metal fabrication industry since 1998, starting his career at the American Welding Society's Welding Journal. Since then he has covered the full range of metal fabrication processes, from stamping, bending, and cutting to grinding and polishing. He joined The Fabricator's staff in October 2007.
- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/07/2024
- Running Time:
- 67:38
Patrick Brunken, VP of Addison Machine Engineering, joins The Fabricator Podcast to talk about the tube and pipe...
- Industry Events
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,