- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Civan Lasers, Fraunhofer ILT, and Smart Move to develop faster bipolar welding feed rate for EV fuel cells
- October 13, 2021
- News Release
- Electric Vehicles
Dynamic beam lasers may provide the automotive industry with a technological solution for economically mass-producing clean-energy engines through increased feed rate for bipolar welding, according to recent findings taking place at the Eureka Project in the Fraunhofer Labs in Aachen, Germany.
As the automotive industry shifts to e-mobility, manufacturers are also shifting from combustion engines to fuel cell engines. The challenge to produce these fuel cells efficiently lies in welding the bipolar plates—thin plates of just hundreds of microns. Each cell contains 300 to 400 of these plates with a weld seam of 3 to 6 m. While there are many efforts to increase the welding speed to keep up with the demand, increasing the feed rate to more than 0.5 m/sec. results in welding defects, leading to faulty parts and a backlog of materials.
The three companies driving the Eureka Project—Civan Lasers in Israel and Germany-based Fraunhofer Institute for Laser Technology ILT and Smart Move—aim to solve this problem by implementing Civan Lasers’ dynamic beam laser technology, which can wobble the beam in microhertz frequencies, creating a faster, more accurate weld of the bipolar plates.
“We look to reach a breakthrough in this project by using advanced sensors and complex beam shapes in high frequencies that were not available in the past,” said Dr. Alexander Olowinsky, researcher from Fraunhofer ILT.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/07/2024
- Running Time:
- 67:38
Patrick Brunken, VP of Addison Machine Engineering, joins The Fabricator Podcast to talk about the tube and pipe...
- Trending Articles
How laser and TIG welding coexist in the modern job shop
Young fabricators ready to step forward at family shop
Material handling automation moves forward at MODEX
A deep dive into a bleeding-edge automation strategy in metal fabrication
Precision Press Brake Certificate Course
- Industry Events
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,