- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
European Commission approves Mittal Steel - Arcelor merger
- June 2, 2006
- News Release
- Metals/Materials
Mittal Steel announced today that the European Commission has cleared its bid to acquire Arcelor subject to certain commitments. The granting of EU antitrust clearance is a further positive and important step towards the successful completion of Mittal's bid, the company said.
"We are delighted with the Commission's decision. For the past several months, we have worked constructively with the Commission— and other regulatory authorities—to demonstrate the pro-competitive impact of the Mittal/Arcelor transaction. Clearly, this decision also recognizes the complementary nature of the combination. The Mittal/Arcelor combination will represent a step-change in the consolidation and long-term health of the global steel industry to the benefit of all stakeholders."
In order to secure clearance during the Commission's Phase I investigation, Mittal Steel agreed to address concerns in what it said is the relatively small area of heavy sections through the divestiture of three steel plants, two belonging to Arcelor and one belonging to Mittal. Mittal Steel believes that the divestitures will have no adverse effect on either company's operations, in light of the combination.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/07/2024
- Running Time:
- 67:38
Patrick Brunken, VP of Addison Machine Engineering, joins The Fabricator Podcast to talk about the tube and pipe...
- Trending Articles
How laser and TIG welding coexist in the modern job shop
Young fabricators ready to step forward at family shop
Material handling automation moves forward at MODEX
A deep dive into a bleeding-edge automation strategy in metal fabrication
Precision Press Brake Certificate Course
- Industry Events
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,