- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
High-strength steel on display with launch of all-new 2019 Ram 1500
- January 16, 2018
- News Release
- Metals/Materials
An interactive steel display is featured in the Ram exhibit at the 2018 North American International Auto Show, running through Jan. 28 at the Cobo Center in Detroit.
The exhibit was designed by the Steel Market Development Institute (SMDI), a business unit of the American Iron and Steel Institute (AISI), in collaboration with Ram. The all-new 2019 Ram 1500 features extensive use of high-strength steel in the cab and frame.
The truck features more than 98 percent high-strength steel in the frame and 54 percent high-strength steel in the core body structure. The use of high-strength steel in the frame reduces noise, vibration, and harshness; saves nearly 225 lbs. of vehicle weight; and provides high rigidity for improved handling and durability, says Ram.
Included in the display are four panels featuring conventional steel, high-strength steel, AHSS, and UHSS. Each removable panel is a different thickness and strength, helping demonstrate to attendees how various grades of steel can be applied to different areas of a vehicle for lightweighting, strength, and occupant protection.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/07/2024
- Running Time:
- 67:38
Patrick Brunken, VP of Addison Machine Engineering, joins The Fabricator Podcast to talk about the tube and pipe...
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,