- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
HRB prices bottoming; down 0.5 percent in U.S., up elsewhere
- August 11, 2010
- News Release
- Metals/Materials
The bi-monthly SteelBenchmarker™ Chinese HRB ex-works price for Aug. 9 rose 2.3 percent to $527 per ton for the second consecutive rise. The Western European HRB price rose 1.8 percent to $690 per ton (on a Euro basis, it rose 1.0 percent), ex-works, for the second consecutive increase. The World export HRB price increased 1.2 percent to $595 per ton, FOB the port of export, for the second consecutive rise. The United States HRB spot price slipped0.5 percent to $634 per metric ton, FOB the mill, for the sixth consecutive decrease.
The four benchmark prices for hot-rolled band for Aug. 9, 2010 are:
- U.S.—$634 per metric ton ($575 per net ton), FOB the mill—down $3 per ton from $637 ($578 net) two weeks ago, and down $142 per ton from the recent high of $776 ($704 net) on May 10, 2010. It is up $205 per ton from the recent low of $429 ($390 net) on May 25, 2009 and down $569 (47.3%) per ton from the record peak of $1,203 ($1,091 net) on July 28, 2008.
- China—$527 per metric ton, ex-works—up $12 per ton from $515 two weeks ago, and down $47 per ton from the recent high of $574 on April 26, 2010. It is up $136 per ton from the recent low of $391 on April 13, 2009 and down $206 (28.1 percent) from the record peak of $733 on July 14, 2008.
- Western Europe—$690 (€5205 per metric ton, ex-works—up $12 per ton from $678 (€520) two weeks ago (on a Euro basis, it was up &eruo;5), down $52 (&eruo;59) per ton from the recent high of $742 (&eruo;584) on May 10, 2010. It is up $237 (€186) from the recent low of $453 (€339) on April 27, 2009 and down $514 (€231) (42.7 percent) per ton from the record peak of $1,204 €756) on July 14, 2008.
- World Export Price—$595 per metric ton, FOB the port of export—up $7 per ton versus $588 two weeks ago, and down $123 per ton from the recent high of $718 on April 26, 2010. It is up $201 per ton from the recent low $394 on May 11, 2009 and down $518 (46.5.2 percent) per ton from the record peak of $1,113 on July 28, 2008.
SteelBenchmarker™ publishes steel benchmark prices for hot-rolled band, cold-rolled coil, rebar and standard plate in the following regions: the U.S., Western Europe, and the world export market. Additionally, there are benchmark prices for steel scrap in the U.S.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/07/2024
- Running Time:
- 67:38
Patrick Brunken, VP of Addison Machine Engineering, joins The Fabricator Podcast to talk about the tube and pipe...
- Industry Events
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,