- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
HRB prices off bottom
- December 16, 2009
- News Release
- Metals/Materials
The bi-monthly SteelBenchmarker™ United States HRB spot price for December 14 rose 4.0 percent to $575 per metric ton, FOB the mill, after four consecutive falls. The World export HRB price rose 3.4 percent to $519 per ton, FOB the port of export, for the second consecutive increase. The Western European HRB price rose 1.1 percent to $577 per ton (on a Euro basis, it rose 3.9 percent), ex-works, after two consecutive declines. The Chinese HRB ex-works price for Dec. 14 rose 0.9 percent to $457 per ton for the fourth consecutive increase.
The four benchmark prices for hot-rolled band for Dec. 14, 2009 are:
- U.S.—$575 per metric ton ($522 per net ton), FOB the mill—up $22 per ton from $553 ($502 net) three weeks ago, and up $146 per ton from recent low of $429 ($390 net) on May 25, 2009. It is down $628 (52.2 percent) per ton from the record peak of $1,203 ($1,091 net) on July 28, 2008 and up $345 per ton from the record low of $230 ($209 net) in December 2001.
- China—$457 per metric ton, ex-works—up $4 per ton from $453 three weeks ago, and up $66 per ton from the recent low of $391 on April 13, 2009. It is down $276 (37.7 percent) per ton from the record peak of $733 on July 14, 2008 and up $210 per ton from the record low of $247 in January 2002.
- Western Europe—$577 (€396) per metric ton, ex-works—up $6 per ton from $571 (€381) three weeks ago (on a Euro basis, up €15), and up $124 (up €57) per ton from the recent low of $453 (€339) on April 27, 2009. It is down $627 (€360) (52.1 percent) per ton from the record peak of $1,204 (€756) on July 14, 2008 and up $388 (€184) per ton from the record low of $189 (€212) in December 2001.
- World Export Price—$519 per metric ton, FOB the port of export—up $17 per ton versus $502 three weeks ago, and up $125 per ton from the recent low of $394 on May 11, 2009. It is down $594 (53.4 percent) per ton from the record peak of $1,113 on July 28, 2008 and up $344 per ton from the record low of $175 in December 2001.
SteelBenchmarker™publishes steel benchmark prices for hot-rolled band, cold-rolled coil, rebar and standard plate in the following regions: the U.S., Western Europe, and the world export market. Additionally, there are benchmark prices for steel scrap in the U.S.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/16/2024
- Running Time:
- 63:29
In this episode of The Fabricator Podcast, Caleb Chamberlain, co-founder and CEO of OSH Cut, discusses his company’s...
- Trending Articles
Tips for creating sheet metal tubes with perforations
JM Steel triples capacity for solar energy projects at Pennsylvania facility
Are two heads better than one in fiber laser cutting?
Supporting the metal fabricating industry through FMA
Omco Solar opens second Alabama manufacturing facility
- Industry Events
16th Annual Safety Conference
- April 30 - May 1, 2024
- Elgin,
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI