- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Copper alloy serves as beryllium-copper alternative
- November 14, 2012
- Product Release
- Metals/Materials
Ampco Metal has introduced AMPCOLOY® 944, a new copper-nickel-silicone-chromium alloy developed as an alternative to beryllium copper for industrial applications requiring a combination of strength and high thermal conductivity. It provides an average hardness of 28 HRC and thermal conductivity of 156 W/m.K.
The alloy can be used for applications demanding a high hardness level, such as cores, core inserts, cavities inserts, runnerless molding systems, hot runner nozzles, core pins, blow pins, ejector-sleeve core combinations, sprue bushings, and neck and tail pinchoffs.
With electrical conductivity of about 35 percent IACS, the alloy can be used in resistance welding applications and integrated circuits chips production fields.
The material is available from stock in round rod diameters from 1 to 4 in. and plate up to 4 in. thick. Other forms available on request include forged shapes and finished-machined parts per customer drawings.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
Why employee-owned companies make sense in manufacturing
What software automation means for custom fabrication
Nucor’s weekly steel price announcement continues to rattle markets
Press brakes, panel benders, and flat blank calculations
Washington artist creates life-size elk sculptures
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,