- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Flaw detector's software simplifies defect sizing
- April 12, 2005
- Product Release
- Testing and Measuring
GE Inspection Technologies' ultrasonic USM 35 flaw detector uses operating software designed to streamline defect sizing in line with API 5UI recommendations for oilfield tubulars.
Using the detector, the operator locates the crack, adjusts the gain to 80 percent amplitude, presses the USM freeze key, and then starts to move the prove to produce an envelope curve. The application software then measures and remembers each amplitude peak and carries out the necessary time of flight calculations for each measurement to provide code-compliant flaw sizing.
Suitable for inspections tasks from flaw detection to corrosion measurement, the detector has two spin and set rotary knobs for setting gain and function values. Direct-access front panel keys are used to select the required dB step width, freeze the displayed A-scan, switch the A-scan to full screen size, and transfer live screen images to an external screen or video projector via a standard VGA output. Instructions are provided in several languages, including most common European languages.
The detector features two independent, color-coded gates with a threshold of 10 percent to 80 percent of screen height that allows two events to be identified and monitored simultaneously. Amplitude for each gate, sound path, or sound path difference can be displayed prominently in the A-scan corner. A high-contrast color display facility also enhances clarity when using angle beam probes in weld inspection. A patented, color-coded leg display allows the signal color to change with sound beam reflection from the workpiece surface. The color display also facilitates highlighting registration curves in DAC and DGS evaluation, filing reference scans, or displaying echo dynamics, because the color can be changed to suit personal preference or ambient light conditions.
High-power lithium ion batteries support the compact detector's portability. They allow at least 10 hours' continuous use and can be recharged while still in the detector. A carrying handle enables positioning the instrument on almost any surface.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/07/2024
- Running Time:
- 67:38
Patrick Brunken, VP of Addison Machine Engineering, joins The Fabricator Podcast to talk about the tube and pipe...
- Industry Events
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,