- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
The Tube and Pipe Journal September 2009
The Tube and Pipe Journal became the first magazine dedicated to serving the metal tube and pipe industry in 1990. Today, it remains the only North American publication devoted to this industry, and it has become the most trusted source of information for tube and pipe professionals.
Shaping profits with a mandrel extractor
- Sep 1, 2009
- Tube and Pipe Fabrication
- Article
Using a mandrel is helpful for maintaining a tubes profile when bending. Without a mandrel, bending forces tend to distort and flatten tubular workpieces.
Manufacturing motorcycle mufflers
- Sep 1, 2009
- Tube and Pipe Fabrication
- Article
Like all manufacturers, Woodsage Industries is always on the lookout for a better way to manufacture the many components it produces for OEMs. It recently devised a way to make one-piece external muffler shells for motorcycles and all-terrain vehicles.
Looking to improve weld seams?
- By Dr. Yehuda Baskin
- Sep 1, 2009
- Tube and Pipe Production
- Article
Most tube and pipe producers weld the seam as it is—without additives or fillers—and risk the problems associated with oxidation. A specially formulated brazing flux, in liquid or paste form, dissolves and removes oxides, prevents re-oxidation, and helps transfer weld heat to the seam.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
Making the move from hard automation to robotic welding
Zekelman Industries to invest $120 million in Arkansas expansion
Brushless copper tubing cutter adjusts to ODs up to 2-1/8 in.
HGG Profiling Equipment names area sales manager
Miscellaneous metals fabricator increases productivity and opportunity with plasma cutting
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,
- Upcoming Webcasts
Navigating Change: The Manufacturer’s Guide to Change Management with ERP Implementation
- May 16, 2024
- Sponsored
- Presented By: ECI Software Solutions, M1
Managing Dangerous Dusts from Metalworking
- June 26, 2024
- Sponsored
- Presented By: Camfil Air Pollution Control