Michigan Tech University Writer
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Our Publications
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Michigan Tech students 3D-print devices to aid arthritis sufferers
‘Anyone who needs an adaptive aid for arthritis should be 3D printing it.’
- By Allison Mills
- December 17, 2018
- Article
- Additive Manufacturing
Excerpted from an article written by Allison Mills that appears on the Michigan Tech website. — Ed.
The Centers for Disease Control and Prevention reports that almost a quarter of the U.S. population lives with some form of arthritis. Daily tasks — like opening drawers, turning door handles — can be difficult, so people turn to adaptive aids. Many are small pieces of plastic.
“It never ceases to amaze me what a small piece of plastic sells for,” said Joshua Pearce, the Richard Witte Endowed Professor of Materials Science and Engineering at Michigan Tech.
Adaptive aids range from $5.99 for a soda-can tab opener to a pill splitter for $23.75 to a phone holder for $49.99. With 3D printing, those costs can come down to 45 cents for a tab popper, $1.27 to split pills and 79 cents plus a rubber band to hold a phone.
“Anyone who needs an adaptive aid for arthritis should be 3D printing it,” said Pearce.
So, he had his class take a shot. Now, Pearce is a co-author and corresponding researcher on a new study that analyzes how 20 of the 3D-printed adaptive aids his class printed provide huge cost savings and either meet — or improve — standards for existing products.
The study was published in Geriatrics journal and is co-authored by student research assistant Nicole Gallup and orthopedic surgeon Jennifer Bow, who is also a visiting scholar at Michigan Tech.
Click here to read the entire article.
About the Author
About the Publication
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Trending Articles
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,