Our Sites
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Our Publications
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
QuesTek’s QT 17-4 powders produce stainless parts that require no high-temp heat treatment
- July 10, 2020
- Product Release
- Additive Manufacturing
QuesTek Innovations LLC has introduced a stainless steel composition for powder bed fusion AM for use either in the as-printed condition or with a single low-temperature heat treatment. This allows for production of complex, high-strength stainless parts via AM, comparable to wrought 17-4 PH, but without the need for cryogenic processing or high-temperature heat treatment.
Two feedstock options are available: QT 17-4 for use in the direct-aged condition and QT 17-4+ for use in the as-printed condition. They can be used in a variety of industries, including aerospace, defense, medical, chemical processing, and energy.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/07/2024
- Running Time:
- 67:38
Patrick Brunken, owner of Addison Machine Engineering, joins The Fabricator Podcast to talk about the tube and pipe...
- Trending Articles
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,