Graduate Research Associate
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Our Publications
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Berk Aykas
Center for Precision Forming at The Ohio State University
1971 Neil Ave. Room 339 Baker Systems Engineering Building
Columbus, OH 43210
- From The Fabricator
R&D Update: Exploring the benefits of servo technology in the pressroom
- By Berk Aykas, David Diaz-Infante, Dr., and Taylan Altan, Ph.D.
- Mar 28, 2019
- Bending and Forming
- Article
CPF researchers employed methods such as variable BHF, cushion pulsation, and attach/detach on a servo press to improve material drawability, reduce springback, and maintain edge quality during blanking.
- From The Fabricator
R&D Update: Using double bending tests to estimate edge fracture occurrence
- By Berk Aykas, David Diaz-Infante, Dr., and Taylan Altan, Ph.D.
- Jan 25, 2019
- Bending and Forming
- Article
Researchers at the Center for Precision Forming share the results of FE simulations to determine an adequate sample size and tooling configuration for the double bend test, used to estimate edge fracture in metal forming.
- From The Fabricator
R&D Update: Practical methods for estimating formability of sheet materials
- By Ali Fallahiarezoodar, Berk Aykas, David Diaz-Infante, Dr., and Taylan Altan, Ph.D.
- Jul 7, 2016
- Bending and Forming
- Article
Formability is the ability of a sheet material to deform without failure or fracture. Information on formability helps process and tool design engineers predict failure during analysis of sheet metal forming processes for tool design. Formability information also is used to evaluate...
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/16/2024
- Running Time:
- 63:29
In this episode of The Fabricator Podcast, Caleb Chamberlain, co-founder and CEO of OSH Cut, discusses his company’s...
- Trending Articles
Tips for creating sheet metal tubes with perforations
Supporting the metal fabricating industry through FMA
JM Steel triples capacity for solar energy projects at Pennsylvania facility
Are two heads better than one in fiber laser cutting?
Zekelman Industries to invest $120 million in Arkansas expansion
- Industry Events
16th Annual Safety Conference
- April 30 - May 1, 2024
- Elgin,
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
- Upcoming Webcasts
Navigating Change: The Manufacturer’s Guide to Change Management with ERP Implementation
- May 16, 2024
- Sponsored
- Presented By: ECI Software Solutions, M1