Graduate Research Assistant, ERC/NSM
Our Sites
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Our Publications
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Giovanni Spampinato
The Ohio State University
1971 Neil Ave. Baker Systems Engineering, Room 339
Columbus, OH
614-292-9267
- From The Fabricator
Warm forming of stainless steels - Part II
- By Ajay Yadav, Giovanni Spampinato, and Taylan Altan, Ph.D.
- Aug 8, 2006
- Metals/Materials
- Article
The ERC/NSM conducted experiments using round cup tooling to determine the influence of temperature on the limiting draw ratio – the largest draw ratio of the blank-to-cup diameter that can be drawn successfully.
- From The Fabricator
Warm forming of stainless steels - Part I
- By Ajay Yadav, Giovanni Spampinato, and Taylan Altan, Ph.D.
- Jul 11, 2006
- Metals/Materials
- Article
To prevent martensitic transformation in stainless steel during drawing operations, warm forming has been explored. In experiments, warm forming eliminated intermediate annealing operations and substantially increased limiting draw ratio values.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/16/2024
- Running Time:
- 63:29
In this episode of The Fabricator Podcast, Caleb Chamberlain, co-founder and CEO of OSH Cut, discusses his company’s...
- Trending Articles
1
Tips for creating sheet metal tubes with perforations
2
JM Steel triples capacity for solar energy projects at Pennsylvania facility
3
Are two heads better than one in fiber laser cutting?
4
Supporting the metal fabricating industry through FMA
5
Zekelman Industries to invest $120 million in Arkansas expansion
- Industry Events
16th Annual Safety Conference
- April 30 - May 1, 2024
- Elgin,
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
- Upcoming Webcasts
Navigating Change: The Manufacturer’s Guide to Change Management with ERP Implementation
- May 16, 2024
- Sponsored
- Presented By: ECI Software Solutions, M1