Graduate Research Associate, ERC/NSM
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Our Publications
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Long Ju
The Ohio State University
1971 Neil Ave. Baker Systems Engineering, Room 339
Columbus, Ohio 43210
614-292-5063
- From The Fabricator
R&D Update: Forming aluminum alloys at elevated temperatures, Part II
- By Taylan Altan, Ph.D. and Long Ju
- Jul 1, 2015
- Bending and Forming
- Article
Elevated-temperature (ET) forming of aluminum can be accomplished isothermally or nonisothermally. In isothermal warm forming, the die, blank holder, and punch are heated. In nonisothermal deep drawing, the die and blank holder are heated, and the punch may or may not be cooled. The die and punch...
- From The Fabricator
R&D Update: Forming aluminum alloys at elevated temperatures, Part 1
- By Taylan Altan, Ph.D. and Long Ju
- Jun 11, 2015
- Bending and Forming
- Article
To reduce vehicle weight, automotive manufacturers are using advanced high-strength steels (AHSS) and aluminum alloys, formed at room temperature, as well as hot stamping of boron steels. A few OEMs and Tier 1 suppliers also have started warm forming aluminum alloys, usually 5000 and 6000 series,...
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/16/2024
- Running Time:
- 63:29
In this episode of The Fabricator Podcast, Caleb Chamberlain, co-founder and CEO of OSH Cut, discusses his company’s...
- Trending Articles
Tips for creating sheet metal tubes with perforations
JM Steel triples capacity for solar energy projects at Pennsylvania facility
Are two heads better than one in fiber laser cutting?
Supporting the metal fabricating industry through FMA
Zekelman Industries to invest $120 million in Arkansas expansion
- Industry Events
16th Annual Safety Conference
- April 30 - May 1, 2024
- Elgin,
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
- Upcoming Webcasts
Navigating Change: The Manufacturer’s Guide to Change Management with ERP Implementation
- May 16, 2024
- Sponsored
- Presented By: ECI Software Solutions, M1