Contributing Writer
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Our Publications
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
- From The Welder
Submerged arc welding : then and now
- By Steven Rainwater
- Jul 29, 2008
- Arc Welding
- Article
Submerged arc welding (SAW) is so named because the weld and arc zone are submerged beneath a blanket of flux. The flux material becomes conductive when it is molten, creating a path for the current to pass between the electrode and the workpiece. The flux blanket prevents spatter and sparks, while...
Better lubricant control leads to better mandrel bends
- By Steven Rainwater
- Sep 11, 2007
- Tube and Pipe Fabrication
- Article
In an effort to reduce the need for cleaning bent tube, fabricator R & B Wagner analyzed its operations and decided to change from manual lubricant application to an automated system. The result was that its lubricant consumption dropped 70 percent. So little lubricant was left on the bent parts that the company eliminated the cleaning step.
- From The Fabricator
Die lubrication: the big picture
- By Steven Rainwater
- Jun 14, 2005
- Bending and Forming
- Article
When considering a die lubrication method, you should be sure to evaluate its effect on your entire operation. While most of us focus on how lubrication affects just the manufacture of parts, a close look reveals that it affects many other aspects of running a plant. However, many of them are not obvious.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/16/2024
- Running Time:
- 63:29
In this episode of The Fabricator Podcast, Caleb Chamberlain, co-founder and CEO of OSH Cut, discusses his company’s...
- Trending Articles
Tips for creating sheet metal tubes with perforations
JM Steel triples capacity for solar energy projects at Pennsylvania facility
Are two heads better than one in fiber laser cutting?
Supporting the metal fabricating industry through FMA
Zekelman Industries to invest $120 million in Arkansas expansion
- Industry Events
16th Annual Safety Conference
- April 30 - May 1, 2024
- Elgin,
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
- Upcoming Webcasts
Navigating Change: The Manufacturer’s Guide to Change Management with ERP Implementation
- May 16, 2024
- Sponsored
- Presented By: ECI Software Solutions, M1