- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Press hardening takes center stage at Schuler convention
- June 18, 2013
- News Release
- Bending and Forming
Press manufacturer Schuler recently held a convention in Waghäusel, Germany, where about 80 visitors heard from industry and academic experts about the latest developments in press hardening and other lightweight construction methods.
Use of press-hardened parts has grown from about 8 million pieces in 1997 to 124 million in 2010. In the next two years, demand is expected to almost quadruple to as many as 450 million pieces. The demand comes mainly from the automotive industry for such parts as bumper supports, roof frames, sills, B-columns, and tunnels.
"Blanks or preformed parts are heated in a furnace to a temperature of 930 degrees C," explained Schuler Sales Manager Jens Aspacher. "The heated blanks then have to be fed into the press as quickly as possible to prevent rapid air cooling." The press remains closed for a few additional seconds during the forming process so that parts can cool and harden. Cycle times are from 8 to 30 sec.
Once they have cooled down, the parts have a final tensile strength of up to 1,500 megapascal. Because of their high rigidity, less material is needed per part to ensure the same level of stability, thus reducing weight. Press force can be reduced to 400 to 1,200 metric tons — as compared to 2,500 to 3,000 metric tons — and springback is reduced.
Related Companies
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,