- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
American Trim, DuPont CoatingSolutions collaborate on coating technology
- February 12, 2008
- News Release
- Finishing
American Trim, Lima, Ohio, has acquired a physical vapor deposition (PVD) chamber designed to allow processing of a chromelike finish without the use of hexavalent chrome and electroplating.
The PVD process uses a base powder coating supplied by DuPont. The powder coating serves as a protective, functional layer and smoothes out the surface. According to American Trim, no sanding or buffing is required on rough parts such as castings. The PVD chamber is utilized to deposit the very thin layer of metal; parts then are coated with a clear acrylic topcoat.
The process is designed primarily for decorative finishing in the heavy-duty truck and automotive industries, American Trim reports. Other applications include appliance, recreational vehicle, furniture, and building products. American Trim will utilize co-branding with DuPont as a member of its Star CoaterSMprogram.
American Trim specializes in the forming, decorating, and coating of metal and composite substrates. DuPont is a provider of science-based products and services.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,