- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
HRB prices down 1.2% to 5.1% in China, Western Europe, U.S., and World
- June 30, 2010
- News Release
- Metals/Materials
The bi-monthly SteelBenchmarker™ Chinese HRB ex-works price for June 28 fell 1.2 percent percent to $511 per ton for the fourth consecutive decrease. The Western European HRB price fell 2.0 percent to $697 per ton (on a Euro basis, it fell 1.6 percent), ex-works, for the third consecutive decline. The United States HRB spot price dropped 2.7 percent to $708 per metric ton, FOB the mill, for the third consecutive decrease. The World export HRB price plunged 5.1 percent to $593 per ton, FOB the port of export, for the fourth consecutive decrease.
The four benchmark prices for hot-rolled band for June 28, 2010 are:
- U.S.—$708 per metric ton ($642 per net ton), FOB the mill—down $20 per ton from $728 ($660 net) two weeks ago, and up $279 per ton from recent low of $429 ($390 net) on May 25, 2009. It is down $495 (41.1 percent) per ton from the record peak of $1,203 ($1,091 net) on July 28, 2008 and up $478 per ton from the record low of $230 ($209 net) in December 2001.
- China—$511 per metric ton, ex-works—down $6 per ton from $517 two weeks ago, and up $120 per ton from the recent low of $391 on April 13, 2009. It is down $222 (30.3 percent) per ton from the record peak of $733 on July 14, 2008 and up $264 per ton from the record low of $247 in January 2002.
- Western Europe—$697 (€571) per metric ton, ex-works—down $14 per ton from $711 (€580) two weeks ago (on a Euro basis, down €9), and up $244 (up €232) per ton from the recent low of $453 €339) on April 27, 2009. It is down $507 €185) (42.1 percent) per ton from the record peak of $1,204 €756) on July 14, 2008 and up $508 €359) per ton from the record low of $189 (€212) in December 2001.
- World Export Price—$593 per metric ton, FOB the port of export—down $32 per ton versus $625 two weeks ago, and up $199 per ton from the recent low of $394 on May 11, 2009. It is down $520 (46.7 percent) per ton from the record peak of $1,113 on July 28, 2008 and up $418 per ton from the record low of $175 in December 2001.
SteelBenchmarker publishes steel benchmark prices for hot-rolled band, cold-rolled coil, rebar and standard plate in the following regions: the U.S., Western Europe, and the world export market. Additionally, there are benchmark prices for steel scrap in the U.S.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,