- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
HRB prices down worldwide
- May 26, 2011
- News Release
- Metals/Materials
The bi-monthly SteelBenchmarker™ Chinese HRB ex-works price for May 23 slipped 0.3 percent to $634 per ton after rising four consecutive times. The World export HRB price slipped 0.5 percent to $728 per ton, FOB the port of export, after rising two weeks ago. The Western European HRB price fell 2.0 percent to $815 per ton (on a Euro basis, it rose 3.0 percent), ex-works, after rising two weeks ago. The United States HRB spot price fell 4.3 percent to $877 per metric ton, FOB the mill, for the fourth consecutive decline.
The four benchmark prices for HRB for May 23, 2011 are:
- U.S.—$877 per metric ton ($796 per net ton), FOB the mill—down $39 per ton from $916 ($831 net) two weeks ago but up $276 per ton from the recent low of $601 ($545 net) on Nov. 8, 2010. It is up $101 per ton from the previous high of $776 ($704 net) on May 10, 2010 and down $326 (27.1 percent) per ton from the record peak of $1,203 ($1,091 net) on July 28, 2008.
- China—$634 per metric ton, ex-works—down $2 per ton from $636 two weeks ago but up $152 per ton from the recent low of $482 on July 12, 2010. It is up $60 per ton from the previous high of $574 on April 26, 2010, but down $99 (13.5 percent) from the record peak of $733 on July 14, 2008.
- Western Europe—$815 (€578 per metric ton, ex-works—down $17 per ton from $832 (€561) two weeks ago (on a Euro basis, it was up €17) and up $147 (€84) per ton from the recent low of $668 (€494) on Nov. 22, 2010. It is up $73 (down €6) from the previous high of $742 (€584) on May 10, 2010 and down $389 (€178) (32.3 percent) per ton from the record peak of $1,204 €756) on July 14, 2008.
- World Export Price—$728 per metric ton, FOB the port of export—down $4 per ton from $732 two weeks ago but up $144 per ton from the recent low of $584 on July 12, 2010. It is up $10 per ton from the previous high of $718 on April 26, 2010, but down $385 (34.6 percent) per ton from the record peak of $1,113 on July 28, 2008.
SteelBenchmarker™ publishes steel benchmark prices for hot-rolled band, cold-rolled coil, rebar and standard plate in the following regions: the U.S., Western Europe, and the world export market. Additionally, there are benchmark prices for steel scrap in the U.S.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,