- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
HRB prices fall 2.3% to 8.6% in Western Europe, China, U.S., and World
- June 17, 2010
- News Release
- Metals/Materials
The bi-monthly SteelBenchmarker™ Western European HRB price for June 14 fell 2.3 percent to $711 per ton (on a Euro basis, it fell 2.5 percent), ex-works, for the second consecutive decline. The Chinese HRB ex-works price dropped 3.2 percent percent to $517 per ton for the third consecutive decrease. The United States HRB spot price dropped 4.2 percent to $728 per metric ton, FOB the mill, for the second consecutive decrease. The World export HRB price plunged 8.6 percent to $625 per ton, FOB the port of export, for the third consecutive decrease.
The four benchmark prices for hot-rolled band for June 14, 2010 are:
- U.S.—$728 per metric ton ($660 per net ton), FOB the mill—down $32 per ton from $760 ($690 net) three weeks ago, and up $299 per ton from recent low of $429 ($390 net) on May 25, 2009. It is down $475 (39.5 percent) per ton from the record peak of $1,203 ($1,091 net) on July 28, 2008 and up $498 per ton from the record low of $230 ($209 net) in December 2001.
- China—$517 per metric ton, ex-works—down $18 per ton from $535 three weeks ago, and up $126 per ton from the recent low of $391 on April 13, 2009. It is down $216 (29.5 percent) per ton from the record peak of $733 on July 14, 2008 and up $270 per ton from the record low of $247 in January 2002.
- Western Europe—$711 (€580) per metric ton, ex-works—down $17 per ton from $728 (€595) three weeks ago (on a Euro basis, down €15), and up $258 (up €241) per ton from the recent low of $453 €339) on April 27, 2009. It is down $493 €176) (40.9 percent) per ton from the record peak of $1,204 €756) on July 14, 2008 and up $522 €368) per ton from the record low of $189 (€212) in December 2001.
- World Export Price—$625 per metric ton, FOB the port of export—down $59 per ton versus $684 three weeks ago, and up $231 per ton from the recent low of $394 on May 11, 2009. It is down $488 (43.8 percent) per ton from the record peak of $1,113 on July 28, 2008 and up $450 per ton from the record low of $175 in December 2001.
SteelBenchmarker publishes steel benchmark prices for hot-rolled band, cold-rolled coil, rebar and standard plate in the following regions: the U.S., Western Europe, and the world export market. Additionally, there are benchmark prices for steel scrap in the U.S.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,