- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
HRB spot steel prices mixed
- April 25, 2007
- News Release
- Metals/Materials
SteelBenchmarker™reported that the U.S. hot-rolled band (HRB) spot price for April 23 dropped 0.8 percent to $625 per metric ton, FOB the mill after five consecutive rises. The world export HRB price slipped 0.3 percent to $589 per ton, FOB the port of export, for the second consecutive drop. The Chinese HRB ex-works price rose 1.8 percent to $448 per ton, for the second consecutive rise. The Western European HRB price rose 2.1 percent to $691 per ton, ex-works, for the 10th time.
The four benchmark prices for hot-rolled band included in the April 23 report are:
- U.S.—$625 per metric ton, FOB the mill—down $5 per ton from $630 two weeks ago and up $54 per ton from the low of $571 on Jan. 22, 2007, but down $73 per ton from the previous high of $698 on July 24, 2006.
- World Export Price—$589 per metric ton, FOB the port of export—down $2 per ton from $591 two weeks ago, but up $90 per ton from the previous low of $499 on Dec. 11, 2006, and down $21 per ton from the peak of $610 on June 12, 2006.
- Western Europe— $691 per metric ton, ex-works—up $14 per ton from $677 two weeks ago and up $135 per ton from the low of $556 on Nov. 27, 2006, and up $60 per ton from the previous peak of $631 reached on July 24, 2006.
- China— $448 per metric ton, ex-works—up $8 per ton from $440 two weeks ago and up $75 per ton from the low of $373 on July 24, 2006, and down $16 per ton from the high of $464 on June 12, 2006.
Twice each month, SteelBenchmarkerpublishes steel benchmark prices for hot-rolled band, cold-rolled coil, rebar, and standard plate in the U.S., Western Europe, mainland China, and the world export market.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,