- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
ITA committee working to remove restrictions on Grade 12 titanium use
- February 9, 2016
- News Release
- Metals/Materials
Denver-based International Titanium Association’s (ITA’s) Industrial Applications Committee has achieved a significant first step in a project to remove restrictions on the use of Grade 12 titanium on NACE MRO 175, a standard for the petroleum and natural gas industries regarding the use and performance of industrial materials in a corrosive, hydrogen-sulfide work environment. The goal is to open up business opportunities for titanium alloy by removing certain restrictions.
The first step to move the project forward involves working with the Corrosion Centre of Exova Group Plc, West Midlands, U.K., which will conduct testing on titanium Grade 12 and present the findings to Houston-based NACE. Nickel alloys currently are the material of choice under the MRO 175 standard for use in hydrogen-sulfide environments for the oil and gas industry.
Applications for titanium Grade 12 in oil and gas production would include valves, pipes, fittings, and heat exchangers. Under MRO 175, such components must be certified to resist “catastrophic cracking” and failure when operating in a corrosive hydrogen-sulfide environment. The standard addresses an industrial material’s ability to withstand stress cracking in a hydrogen-sulfide environment, also known as a sour service or sour gas environment.
While titanium Grade 12, an alloy that includes nickel and molybdenum, is resistant to hydrogen-sulfide industrial environments, it currently is “not in harmony” with the MRO 175 standard, originally written in the 1980s, in areas such as basic mill practices, plate hardness, and heat-treating techniques, ITA reports. The association believes updating requirements for the production of Grade 12 titanium under the MRO 175 specification will have a positive effect on the global titanium industry.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,