- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
LIFT project to focus on computer analytics to predict titanium performance
- January 19, 2016
- News Release
- Metals/Materials
The third technology project announced by Detroit-based LIFT (Lightweight Innovations for Tomorrow) will focus on titanium. Lead partners on the project—GE Aviation and The Ohio State University—will focus first on advancing computer analytics to better understand and predict the performance of titanium alloys.
“Titanium is expensive, and engineers have to ‘make and break’ a lot of test parts before they can be sure the design is right for a critical component of an airplane engine,” said Alan Taub, chief technology officer at LIFT. “If we can advance the abilities of our computer models to better predict how a particular design will perform, we can test less. That cuts material and testing costs and the lead time for developing new designs.”
Thomas F. Broderick, senior staff engineer, structural materials development, GE Aviation, said, "Our interests emphasize development of computational means to predict fatigue and ballistic impact resistance within the highly transformed microstructures that are formed about the solid-state weld interface.”
Boeing and Scientific Forming Technologies Corp. are the other industry partners on the project. EWI, Purdue University, Southwest Research Institute, University of Michigan, and the University of North Texas will contribute to the project as research participants.
“This project aims to develop computer models that will reduce by 50 percent both the time and cost for materials development, component design, and manufacture,” said Taub. “In addition, the new computational tools will help us manufacture components that perform better.
LIFT is operated by the American Lightweight Materials Manufacturing Innovation Institute (ALMMII) and was selected through a competitive process led by the U.S. Department of Defense under the Lightweight and Modern Metals Manufacturing Innovation (LM3I) solicitation issued by the U.S. Navy's Office of Naval Research.
LIFT is one of the founding institutes in the National Network for Manufacturing Innovation, a federal initiative to create regional hubs to accelerate the development and adoption of cutting-edge manufacturing technologies.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,