- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
New ASTM standard supports use of steel heat-treated by the induction method
- December 15, 2016
- News Release
- Metals/Materials
A new ASTM Intl. standard will help those who both provide and use induction heat treatment to strengthen metals. While guides and specifications already exist to qualify standard heat-treating furnaces, this new standard will be the first generally accepted guide for qualification of induction heat treating, which heats metal electronically by passing it through a series of coils.
A1100, Guide for Qualification and Control of Induction Heat Treating was developed by ASTM’s committee on steel, stainless steel, and related alloys (A01).
According to ASTM member Lester Burgess, director of technical services and quality at TSP/US Bolt Mfg., the guide will help induction heat-treatment providers to define and accomplish needed internal qualification and control of processes. The guide will also allow users to better qualify and confirm the competency of providers. Other stakeholders will find the guide useful as an auditing process for evaluating providers.
To purchase standards, visit www.astm.org and search by the standard designation, or contact ASTM customer relations at 877-909-2786 or sales@astm.org.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,