- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
New standards released for metal powder testing, bearings
- February 9, 2010
- News Release
- Metals/Materials
New 2010 editions of two powder metallurgy (PM) standards have been issued by the Metal Powder Industries Federation (MPIF).
The 130-page Standard Test Methods for Metal Powders and Powder Metallurgy Products contains 39 individual standards on terminology and recommended methods for testing metal powders, PM parts, metal injection molded (MIM) parts, metallic filters, and PM equipment. In addition to a new standard on sample preparation for the determination of the total carbon content of PM materials (excluding cemented carbides), the new edition features revisions on 10 standards.
The 28-page Standard 35, Materials Standards for PM Self-Lubricating Bearings, has a new material section on diffusion-alloyed iron-bronze bearings; new information on oil impregnation efficiency; revised information for bronze bearings; and data table modifications.
Both editions cross-reference comparable ASTM and ISO standards.
The standards are available for a fee in soft-cover, electronic, and CD-ROM formats.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,