- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
North American aluminum industry makes big sustainability gains, study says
- January 14, 2014
- News Release
- Metals/Materials
Energy demand and greenhouse gas emissions associated with primary aluminum production in the U.S. and Canada have declined significantly in recent years, according to a new, peer-reviewed life-cycle assessment (LCA) report released by the Aluminum Association, Arlington, Va. The study found major improvements, particularly in terms of more sustainable production, in all life cycle impacts, from aluminum production through semifabrication.
According to the report, the energy needed to produce a single metric ton of primary (new) aluminum has declined 11 percent since 2005 and 26 percent since 1995. The industry's carbon footprint has fallen 19 percent since 2005 and 37 percent since 1995. A voluntary effort undertaken by the industry in the early 1990s with the U.S. EPA has reduced emissions of perfluorocarbons (PFC), a greenhouse gas, by nearly 85 percent.
The new findings are based on a multiyear LCA study examining the environmental impact of modern aluminum production. The study reviewed the 2010 production year and incorporates data from 25 companies, representing 95 percent of primary metal production and the majority of the industry in the U.S. and Canada. The report includes data on every aspect of primary and secondary aluminum production, as well as semifabrication.
Technological advances in the aluminum production process are the primary drivers of the environmental improvements realized by the industry. These advances include:
- * The increased use of computerized process controls to lower electric power usage needed to produce primary aluminum.
- * The gradual phaseout of older facilities relying on more energy-intensive production processes.
- * The expanded use of renewable hydroelectric power sources for aluminum production, which has risen from 63 percent in 1995 to 75 percent today.
To learn more and read the complete report, visit www.aluminum.org/lcareport.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/16/2024
- Running Time:
- 63:29
In this episode of The Fabricator Podcast, Caleb Chamberlain, co-founder and CEO of OSH Cut, discusses his company’s...
- Trending Articles
Tips for creating sheet metal tubes with perforations
Supporting the metal fabricating industry through FMA
JM Steel triples capacity for solar energy projects at Pennsylvania facility
Fabricating favorite childhood memories
Omco Solar opens second Alabama manufacturing facility
- Industry Events
16th Annual Safety Conference
- April 30 - May 1, 2024
- Elgin,
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI