- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Stainless tube imports surging from China and Korea
- January 6, 2015
- News Release
- Metals/Materials
Imports of seamless stainless steel tube from China and Korea are surging into the U.S. market, according to the Stainless Steel Tube Trade Advancement Committee (SSTTAC).
"Imports from China through October 2014 have doubled over the same period last year based on U.S. government official trade data," said David A. Hartquist, counsel to the SSTTAC and a partner in the law firm Kelley Drye & Warren, Washington, D.C. “The average unit value of the Chinese imports is by far the lowest of all significant exporters to the U.S. This raises a question as to whether the Chinese product is being dumped in our market. Imports from Korea also are up substantially, increasing by 49 percent over the same period in 2013. The SSTTAC will continue its active monitoring of such imports and determine what actions should be taken."
The SSTTAC, which comprises U.S. producers of seamless stainless steel pipe and tube, promotes domestic manufacturing of high-quality seamless stainless steel tubing. Member companies produce tubing to industry and consumer specifications in accordance with guidelines and requirements of accreditation societies.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,