- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Steel prices predicted to remain high
- January 31, 2006
- News Release
- Metals/Materials
Rising steel prices have caused pain for many U.S. industries and significant relief is not on the horizon, Roland Berger Strategy Consultants said today.
Since 2003 steel prices have climbed by more than 150 percent. Hot-rolled coil prices—a benchmark for pricing—reached a record high of $756 per ton in September 2004 and averaged $744 per ton in 2005.
The recent spike in prices was caused by several factors, including increased consumption by China and India; recent consolidation within the U.S. steel industry; and continued growth in demand for steel in the U.S.
Over the past decade, China's consumption of steel has doubled. In 2005, it accounted for 30 percent of global demand. "China is now the largest consumer of steel in the world," noted Wim van Acker, managing partner, Roland Berger Strategy Consultants, North America.
Industry consolidation also has played a role in rising prices. In 2002 steel prices were depressed, averaging just $319 per ton. Seven steel companies controlled approximately 53 percent of the U.S. market, and there was substantial overcapacity. A wave of bankruptcies, mergers and acquisitions followed.
By 2006 three companies—Mittal, U.S. Steel, and Nucor—controlled a combined 55 percent of the U.S. market.
"The proposed acquisition of Arcelor by Mittal will have a minimal impact in the U.S., but will further increase consolidation globally," said Antonio Benecchi, partner, Roland Berger Strategy Consultants, North America.
Demand for steel in construction is expected to remain high in 2006 and automotive steel consumption, led by sport-utility vehicles and automotive transplants also has been rising. After falling during the 1970s and 1980s, the popularity of SUVs caused automotive steel use to increase seven percent to 1,842 pounds per vehicle between 1990 and 2004. Transplant automobile manufacturers also are contributing to rising demand, with an expectation that they will increase domestic vehicle production 12 percent between 2005 and 2007.
"Today, steel companies have gone from being price takers in a competitive market to price setters with their customers," Benecchi noted.
Roland Berger expects prices to remain relatively high in 2006 and 2007. Prices for 2006 are forecast to be between $500 and $550 a ton. With no catalysts for significant price reductions in sight, prices in 2007 may decline somewhat from 2006 levels, but will remain historically high.
"The price increases in 2004 and 2005 were historically significant," said van Acker. "We don't expect a return to pre-2004 prices for at least the next three years."
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,