- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
World, U.S., Western Europe hot-rolled band prices decline
- August 30, 2006
- News Release
- Metals/Materials
SteelBenchmarker™reported that the hot-rolled band (HRB) world export price for Aug. 28 declined $16 per ton to $554 per ton from $570 per ton, FOB the port of export, on Aug. 14. The U.S. spot price fell to $680 per ton from $687 per ton on Aug. 14.
The four benchmark prices for hot-rolled band included in the report are:
- U.S. — $680 per metric ton, FOB the mill (down $7 per ton, or 1%, from $687 two weeks ago, but still up $62 per ton, or 10%, from April 10).
- World Export Price — $554 per metric ton, FOB the port of export (down $16 per ton, or 3%, versus $570 on Aug. 14, but up $37 per ton, or 7%, since April).
- Western Europe — $609 per metric ton, FOB the port of export (down $22 per ton, or 3.5%, versus $631 on July 24, but up $11 per ton, or 2%, since May 8.
- China — $379 per metric ton, ex-works (up $2 per ton, or 0.5%, from $377 two weeks ago, but still down $23 per ton, or 6% since April 10).
Twice each month, SteelBenchmarkerpublishes steel benchmark prices for hot-rolled band, cold-rolled coil, rebar, and standard plate in the U.S., Western Europe, mainland China, and the world export market.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,