- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
Retaining compounds cure through contaminants
- October 22, 2013
- Product Release
- Assembly and Joining
Henkel Corp. has announced enhancements to three Loctite® anaerobic retaining compounds to allow primerless performance on oily or contaminated surfaces at operating temperatures as high as 356 degrees F.
Loctite 638™ is a general-purpose retaining compound recommended for press fits that need subsequent disassembly. Designed for use on loose-fitting parts, the high-strength adhesive resists temperatures to 347 degrees F and can be used on applications with larger gaps approaching 0.009 in. The adhesive is registered to NSF Category P1.
Loctite 648™ is a high-strength retaining compound recommended for continuous working temperatures to 356 degrees F. This general-purpose retaining adhesive fixtures in 5 min., with full cure in 24 hours, and is designed for use on close-fitting parts. The high-strength formulation bonds to stainless steel press and interference fits and fills gaps to 0.006 in. The adhesive is certified to ANSI/NSF Standard 61 for use in potable water systems.
Loctite 680™ is a high-strength retaining adhesive for use on slip-fitted parts with gaps as large as 0.014 in. This low-viscosity material is certified to ANSI/NSF Standard 61 for use in potable water systems.
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 04/30/2024
- Running Time:
- 53:00
Seth Feldman of Iowa-based Wertzbaugher Services joins The Fabricator Podcast to offer his take as a Gen Zer...
- Industry Events
Pipe and Tube Conference
- May 21 - 22, 2024
- Omaha, NE
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,